Complete Set of CAMPUS® Data, ASTM Data, Biopolymer Database, Application Database, Tradename Database, Literature Database, Toolbox.

Material datasheets available free. Online registration at: www.materialdatacenter.com

Material Data Center is a leading international information system for the plastics industry. Material Data Center offers a comprehensive plastics database, calculation tools, CAE interfaces, a literature database and an application database. For more information about Material Data Center visit www.materialdatacenter.com.

This is the free Material Data Center Datasheet of Kynar Flex® 2751-00 - PVDF - ARKEMA

Material Data Center offers the following functions for Kynar Flex® 2751-00:
unit conversion, PDF datasheet print, comparison with other plastics, snap fit calculation, beam deflection calculation, CAE Interfaces

Check here, which other Kynar Flex datasheets, application examples or technical articles are available in Material Data Center

Use the following short links to get directly to the properties of interest in this datasheet:
Any use of this information falls under the rules of our disclaimer.
Testo del prodotto
Kynar Flex® resins are fluorinated thermoplastic copolymers.

Outstanding characteristics: chemical resistance, imperviousness to UV, barrier properties and high purity.

Kynar Flex® 2751-00 resin is a powder grade where maximum flexibility or impact strength is required.


Main applications:
  • flexible tubing
  • corrosion protection in the chemical industry
  • off-shore
  • wire and cable
Caratteristiche FisicheValoreUnitáNorma del test
ISO Data
Indice di fusione di volume, MVR 1.9 cm³/10min ISO 1133
Temperatura 230 °C -
Carico 5 kg -
Proprietà MeccanicheValoreUnitáNorma del test
ISO Data
Modulo a trazione 450 MPa ISO 527
Carico unitario a trazione 21 MPa ISO 527
Deformazione a snervamento 15 % ISO 527
Deformazione nominale a rottura >50 % ISO 527
Proprietà TermicheValoreUnitáNorma del test
ISO Data
Temperatura di fusione, 10°C/min 134 °C ISO 11357-1/-3
Temperatura di transizione vetrosa, 10°C/min -40 °C ISO 11357-1/-2
Temp.di inflessione sotto carico, 1.80 MPa 40 °C ISO 75-1/-2
Reazione al fuoco a spessore h V-0 class IEC 60695-11-10
Spessore provato 0.8 mm -
Indice di ossigeno 43 % ISO 4589-1/-2
Proprietà ElettricheValoreUnitáNorma del test
ISO Data
Resistività volumica 2E12 Ohm*m IEC 62631-3-1
Caratteristiche
Forma fisica disponibile
Polveri
Caratteristiche
Copolimero
Disponibilità geografica
Disclaimer
Copyright Altair Engineering GmbH. Altair Engineering GmbH assumes no liability for the system to be free of errors. The user takes sole responsibility for the use of this data under the exclusion of every liability from Altair Engineering GmbH; this is especially valid for claims of compensation resulting from consequential damages. Altair explicitly points out that any decision about the application of materials must be double checked with the producer of this material. This includes all contents of this system. Copyright laws are applicable for the content of this system.
Created: Source: www.materialdatacenter.com


Material Data Center is provided by M-Base Engineering + Software GmbH. M-Base Engineering + Software GmbH assumes no liability for the system to be free of errors. Any decision about the application of materials must be double checked with the producer of this material.

Additional information about this material, like producer contact address, etc. can be found at www.materialdatacenter.com. For access to this extra information a registration is requested. Free online registration is available.